产品展厅
![]() |
高模敷PA6 东丽 CM1011RG-02 玻璃45%强化 通用
- 品牌:东丽
- 货号:125
- 价格: ¥14.5/千克
- 发布日期: 2022-09-08
- 更新日期: 2025-06-23
产品详请
品牌 | 东丽 |
货号 | 125 |
用途 | 通用 |
牌号 | CM1011RG-02 |
型号 | CM1011RG-02 |
品名 | PA6 |
外形尺寸 | 袋装 |
生产企业 | 东丽 |
是否进口 | 否 |
PA6 日本东丽 CM1011RG-02 注塑级
特性
特性:玻璃45%强化,高模敷
断裂伸长率
23℃
ASTM D-638
无水|5
%
23℃
ASTM D-638
1.9%水|5
%
抗剪强度
23℃
ASTM D-732
无水|940
kg/cm2
23℃
ASTM D-732
1.9%水|750
kg/cm2
抗拉屈服强度
23℃
ASTM D-638
无水|2000
kg/cm2
23℃
ASTM D-638
1.9%水|1300
kg/cm2
80℃
ASTM D-638
无水|1200
kg/cm2
80℃
ASTM D-638
1.9%水|-
kg/cm2
-40℃
ASTM D-638
无水|2900
kg/cm2
-40℃
ASTM D-638
1.9%水|-
kg/cm2
洛氏硬度
23℃
ASTM D-785
1.9%水|-
R-标度
23℃
ASTM D-785
无水|95
M-标度
23℃
ASTM D-785
1.9%水|-
M-标度
23℃
ASTM D-785
无水|121
R-标度
挠曲模量
23℃
ASTM D-790
无水|122000
kg/cm2
23℃
ASTM D-790
1.9%水|72000
kg/cm2
80℃
ASTM D-790
无水|63000
kg/cm2
80℃
ASTM D-790
1.9%水|45000
kg/cm2
-40℃
ASTM D-790
无水|140000
kg/cm2
-40℃
ASTM D-790
1.9%水|120000
kg/cm2
挠曲强度
23℃
ASTM D-790
无水|2900
kg/cm2
23℃
ASTM D-790
1.9%水|1850
kg/cm2
80℃
ASTM D-790
无水|16000
kg/cm2
80℃
ASTM D-790
1.9%水|-
kg/cm2
-40℃
ASTM D-790
无水|3300
kg/cm2
-40℃
ASTM D-790
1.9%水|-
kg/cm2
压缩强度
23℃
ASTM D-695
无水|1900
kg/cm2
23℃
ASTM D-695
1.9%水|-
kg/cm2
80℃
ASTM D-695
无水|1000
kg/cm2
80℃
ASTM D-695
1.9%水|-
kg/cm2
-40℃
ASTM D-695
无水|2600
kg/cm2
-40℃
ASTM D-695
1.9%水|-
kg/cm2
IZOD冲击强度
23℃,无缺口1/8
ASTM D-256
1.9%水|120
kg·cm/cm
-40℃,无缺口1/8
ASTM D-256
无水|12.5
kg·cm/cm
-40℃,无缺口1/8
ASTM D-256
1.9%水|15
kg·cm/cm
-40℃,无缺口1/8
ASTM D-256
无水|12.5
kg·cm/cm2
-40℃,无缺口1/8
ASTM D-256
1.9%水|15
kg·cm/cm2
23℃,V缺口1/2
ASTM D-256
无水|15
kg·cm/cm
23℃,V缺口1/2
ASTM D-256
1.9%水|20
kg·cm/cm
23℃,无缺口1/8
ASTM D-256
无水|98
kg·cm/cm
热性能
测试条件
测试方法
测试结果
单位
UL-94抗燃级
1/32"
UL 94
无水|HB
1/32"
UL 94
1.9%水|-
比热
无水|0.31
Cal/g·℃
1.9%水|-
Cal/g·℃
热挠曲温度
4.6kg/cm2
ASTM D-648
无水|225
℃
4.6kg/cm2
ASTM D-648
1.9%水|-
℃
熔点
差示扫描测热计DSC
无水|225
℃
差示扫描测热计DSC
1.9%水|-
℃
线性热膨胀系数
ASTM D-696
无水|2-3
×10-5cm/cm/℃
ASTM D-696
1.9%水|-
×10-5cm/cm/℃
电气性能
测试条件
测试方法
测试结果
单位
介电常数
106Hz
ASTM D-150
无水|4.2
106Hz
ASTM D-150
1.9%水|4.5
103Hz
ASTM D-150
无水|4.9
103Hz
ASTM D-150
1.9%水|7.4
介电强度
1/8"
ASTM D-149
无水|19
KV/mm
1/8"
ASTM D-149
1.9%水|15
KV/mm
抗电弧性
1/8"
ASTM D-495
无水|104
S
1/8"
ASTM D-495
1.9%水|119
S
损耗因数
50Hz
ASTM D-150
无水|0.03
50Hz
ASTM D-150
1.9%水|0.16
106Hz
ASTM D-150
无水|0.02
106Hz
ASTM D-150
1.9%水|0.06
体积电阻率
ASTM D-257
无水|1015
Ω.cm
ASTM D-257
1.9%水|1012
Ω.cm
、
PA6 日本东丽 CM1011RG-02 注塑级
特性 | 特性:玻璃45%强化,高模敷 |
断裂伸长率 | 23℃ | ASTM D-638 | 无水|5 | % |
23℃ | ASTM D-638 | 1.9%水|5 | % | |
抗剪强度 | 23℃ | ASTM D-732 | 无水|940 | kg/cm2 |
23℃ | ASTM D-732 | 1.9%水|750 | kg/cm2 | |
抗拉屈服强度 | 23℃ | ASTM D-638 | 无水|2000 | kg/cm2 |
23℃ | ASTM D-638 | 1.9%水|1300 | kg/cm2 | |
80℃ | ASTM D-638 | 无水|1200 | kg/cm2 | |
80℃ | ASTM D-638 | 1.9%水|- | kg/cm2 | |
-40℃ | ASTM D-638 | 无水|2900 | kg/cm2 | |
-40℃ | ASTM D-638 | 1.9%水|- | kg/cm2 | |
洛氏硬度 | 23℃ | ASTM D-785 | 1.9%水|- | R-标度 |
23℃ | ASTM D-785 | 无水|95 | M-标度 | |
23℃ | ASTM D-785 | 1.9%水|- | M-标度 | |
23℃ | ASTM D-785 | 无水|121 | R-标度 | |
挠曲模量 | 23℃ | ASTM D-790 | 无水|122000 | kg/cm2 |
23℃ | ASTM D-790 | 1.9%水|72000 | kg/cm2 | |
80℃ | ASTM D-790 | 无水|63000 | kg/cm2 | |
80℃ | ASTM D-790 | 1.9%水|45000 | kg/cm2 | |
-40℃ | ASTM D-790 | 无水|140000 | kg/cm2 | |
-40℃ | ASTM D-790 | 1.9%水|120000 | kg/cm2 | |
挠曲强度 | 23℃ | ASTM D-790 | 无水|2900 | kg/cm2 |
23℃ | ASTM D-790 | 1.9%水|1850 | kg/cm2 | |
80℃ | ASTM D-790 | 无水|16000 | kg/cm2 | |
80℃ | ASTM D-790 | 1.9%水|- | kg/cm2 | |
-40℃ | ASTM D-790 | 无水|3300 | kg/cm2 | |
-40℃ | ASTM D-790 | 1.9%水|- | kg/cm2 | |
压缩强度 | 23℃ | ASTM D-695 | 无水|1900 | kg/cm2 |
23℃ | ASTM D-695 | 1.9%水|- | kg/cm2 | |
80℃ | ASTM D-695 | 无水|1000 | kg/cm2 | |
80℃ | ASTM D-695 | 1.9%水|- | kg/cm2 | |
-40℃ | ASTM D-695 | 无水|2600 | kg/cm2 | |
-40℃ | ASTM D-695 | 1.9%水|- | kg/cm2 | |
IZOD冲击强度 | 23℃,无缺口1/8 | ASTM D-256 | 1.9%水|120 | kg·cm/cm |
-40℃,无缺口1/8 | ASTM D-256 | 无水|12.5 | kg·cm/cm | |
-40℃,无缺口1/8 | ASTM D-256 | 1.9%水|15 | kg·cm/cm | |
-40℃,无缺口1/8 | ASTM D-256 | 无水|12.5 | kg·cm/cm2 | |
-40℃,无缺口1/8 | ASTM D-256 | 1.9%水|15 | kg·cm/cm2 | |
23℃,V缺口1/2 | ASTM D-256 | 无水|15 | kg·cm/cm | |
23℃,V缺口1/2 | ASTM D-256 | 1.9%水|20 | kg·cm/cm | |
23℃,无缺口1/8 | ASTM D-256 | 无水|98 | kg·cm/cm | |
热性能 | 测试条件 | 测试方法 | 测试结果 | 单位 |
---|---|---|---|---|
UL-94抗燃级 | 1/32" | UL 94 | 无水|HB | |
1/32" | UL 94 | 1.9%水|- | ||
比热 | 无水|0.31 | Cal/g·℃ | ||
1.9%水|- | Cal/g·℃ | |||
热挠曲温度 | 4.6kg/cm2 | ASTM D-648 | 无水|225 | ℃ |
4.6kg/cm2 | ASTM D-648 | 1.9%水|- | ℃ | |
熔点 | 差示扫描测热计DSC | 无水|225 | ℃ | |
差示扫描测热计DSC | 1.9%水|- | ℃ | ||
线性热膨胀系数 | ASTM D-696 | 无水|2-3 | ×10-5cm/cm/℃ | |
ASTM D-696 | 1.9%水|- | ×10-5cm/cm/℃ | ||
电气性能 | 测试条件 | 测试方法 | 测试结果 | 单位 |
介电常数 | 106Hz | ASTM D-150 | 无水|4.2 | |
106Hz | ASTM D-150 | 1.9%水|4.5 | ||
103Hz | ASTM D-150 | 无水|4.9 | ||
103Hz | ASTM D-150 | 1.9%水|7.4 | ||
介电强度 | 1/8" | ASTM D-149 | 无水|19 | KV/mm |
1/8" | ASTM D-149 | 1.9%水|15 | KV/mm | |
抗电弧性 | 1/8" | ASTM D-495 | 无水|104 | S |
1/8" | ASTM D-495 | 1.9%水|119 | S | |
损耗因数 | 50Hz | ASTM D-150 | 无水|0.03 | |
50Hz | ASTM D-150 | 1.9%水|0.16 | ||
106Hz | ASTM D-150 | 无水|0.02 | ||
106Hz | ASTM D-150 | 1.9%水|0.06 | ||
体积电阻率 | ASTM D-257 | 无水|1015 | Ω.cm | |
ASTM D-257 | 1.9%水|1012 | Ω.cm |